Study of creep deformation of irradiated zircaloy cladding by isothermal heating of irradiated PHWR fuel pins in temperature range 700oC-900oC
dc.contributor.author | Sah, D. N. | |
dc.contributor.author | Viswanathan, U. K. | |
dc.contributor.author | Anantharaman, S. | |
dc.date.accessioned | 2011-05-05T04:14:13Z | |
dc.date.available | 2011-05-05T04:14:13Z | |
dc.date.issued | 2010 | |
dc.format.extent | 4666 bytes | |
dc.format.mimetype | text/html | |
dc.identifier.source | Transactions of the Indian Institute of Metals. Vol. 63 (2-3): pp. 467-471 | en |
dc.identifier.uri | http://hdl.handle.net/123456789/4580 | |
dc.language.iso | en | en |
dc.subject | PHWR fuel | en |
dc.subject | accident behaviour | en |
dc.subject | high temperature creep | en |
dc.subject | ballooning | en |
dc.subject | loss of coolant accident (LOCA) | en |
dc.title | Study of creep deformation of irradiated zircaloy cladding by isothermal heating of irradiated PHWR fuel pins in temperature range 700oC-900oC | en |