Rupture behaviour of nuclear fuel cladding during loss-of-coolant accident
dc.contributor.author | Suman, S. | |
dc.contributor.author | Khan, M. K. | |
dc.contributor.author | Pathak, M. | |
dc.contributor.author | Singh, R. N. | |
dc.contributor.author | Chakravartty, J. K. | |
dc.date.accessioned | 2017-01-17T06:07:05Z | |
dc.date.available | 2017-01-17T06:07:05Z | |
dc.date.issued | 2016 | |
dc.description.division | MMD | en |
dc.format.extent | 4220 bytes | |
dc.format.mimetype | text/html | |
dc.identifier.source | Nuclear Engineering and Design, 2016. Vol. 307: pp. 319-327 | en |
dc.identifier.uri | http://hdl.handle.net/123456789/13955 | |
dc.language.iso | en | en |
dc.subject | Materials Engineering | en |
dc.subject | Rupture behaviour | en |
dc.subject | nuclear fuel cladding | en |
dc.subject | loss-of-coolant accident | en |
dc.title | Rupture behaviour of nuclear fuel cladding during loss-of-coolant accident | en |
dc.type | Article | en |