Effect of structural defects, surface irregularities, and quenched-in defects on corrosion of Zr-based metallic glasses
dc.contributor.author | Vishwanadh, B. | |
dc.contributor.author | Abraham, G. J. | |
dc.contributor.author | Jagannath | |
dc.contributor.author | Neogy, S. | |
dc.contributor.author | Dutta, R. S. | |
dc.contributor.author | Dey, G. K. | |
dc.date.accessioned | 2010-08-19T09:05:35Z | |
dc.date.available | 2010-08-19T09:05:35Z | |
dc.date.issued | 2009 | |
dc.format.extent | 4542 bytes | |
dc.format.mimetype | text/html | |
dc.identifier.uri | http://hdl.handle.net/123456789/3615 | |
dc.language.iso | en | en |
dc.subject | structural defects | en |
dc.subject | surface irregularities | en |
dc.subject | quenched-in defects | en |
dc.subject | corrosion | en |
dc.subject | Zr-based metallic glasses | en |
dc.title | Effect of structural defects, surface irregularities, and quenched-in defects on corrosion of Zr-based metallic glasses | en |
dc.type | Article | en |