Delayed hydride cracking in Zr–2.5Nb pressure tube material
dc.contributor.author | Singh, R. N. | |
dc.contributor.author | Niraj Kumar | |
dc.contributor.author | Kishore, R. | |
dc.contributor.author | Roychaudhury, S. | |
dc.contributor.author | Sinha, T. K. | |
dc.date.accessioned | 2019-09-12T09:07:54Z | |
dc.date.available | 2019-09-12T09:07:54Z | |
dc.date.issued | 2002 | |
dc.description.division | MSD | en |
dc.format.extent | 4145 bytes | |
dc.format.mimetype | text/html | |
dc.identifier.source | Journal of Nuclear Materials, 2002. Vol. 304: pp. 189-203 | en |
dc.identifier.uri | http://hdl.handle.net/123456789/19352 | |
dc.language.iso | en | en |
dc.subject | Delayed hydride cracking | en |
dc.subject | Zr–2.5Nb pressure tube material | en |
dc.subject | tensile stress gradient | en |
dc.subject | DHC velocity | en |
dc.title | Delayed hydride cracking in Zr–2.5Nb pressure tube material | en |
dc.type | Article | en |