Effect of uranium oxide loading on the enthalpy increment (DH) and heat capacity (Cp) values of modified borosilicate glass for radwaste immobilisation
dc.contributor.author | Praveena, N. | |
dc.contributor.author | Maji, B. K. | |
dc.contributor.author | Jena, H. | |
dc.date.accessioned | 2020-11-12T09:09:50Z | |
dc.date.available | 2020-11-12T09:09:50Z | |
dc.date.issued | 2019 | |
dc.description.division | BARCF-K | en |
dc.format.extent | 4129 bytes | |
dc.format.mimetype | text/html | |
dc.identifier.source | Journal of Thermal Analysis and Calorimetry, 2019. Vol. 136: pp. 697-701 | en |
dc.identifier.uri | http://hdl.handle.net/123456789/21333 | |
dc.language.iso | en | en |
dc.subject | Borosilicate glass | en |
dc.subject | Nuclear waste | en |
dc.subject | Enthalpy increment | en |
dc.subject | Heat capacity | en |
dc.subject | DSC method | en |
dc.title | Effect of uranium oxide loading on the enthalpy increment (DH) and heat capacity (Cp) values of modified borosilicate glass for radwaste immobilisation | en |
dc.type | Article | en |