Transferability of specimen J-R curve to straight pipe with circumferential surface flaw
dc.contributor.author | Sahu, M. K. | |
dc.contributor.author | Chattopadhyay, J. | |
dc.contributor.author | Dutta, B. K. | |
dc.date.accessioned | 2012-08-23T08:44:51Z | |
dc.date.available | 2012-08-23T08:44:51Z | |
dc.date.issued | 2012 | |
dc.description.division | RSD | en |
dc.format.extent | 5242 bytes | |
dc.format.mimetype | text/html | |
dc.identifier.source | Fatigue & Fracture of Engineering Materials & Structures, 2012. Vol. 35 (5): pp. 476-487 | en |
dc.identifier.uri | http://hdl.handle.net/123456789/6535 | |
dc.language.iso | en | en |
dc.subject | crack-tip constraint | en |
dc.subject | fracture | en |
dc.subject | J–R curve | en |
dc.subject | stress triaxiality factor | en |
dc.subject | pipe | en |
dc.subject | transferability | en |
dc.title | Transferability of specimen J-R curve to straight pipe with circumferential surface flaw | en |
dc.type | Article | en |