Threshold stress intensity factor for delayed hydride cracking in Zr-2. 5%Nb pressure tube alloy

dc.contributor.authorSingh, R. N.
dc.contributor.authorStahle, P.
dc.contributor.authorChakravartty, J. K.
dc.contributor.authorShmakov, A. A.
dc.date.accessioned2010-08-20T08:24:22Z
dc.date.available2010-08-20T08:24:22Z
dc.date.issued2009
dc.format.extent4000 bytes
dc.format.mimetypetext/html
dc.identifier.urihttp://hdl.handle.net/123456789/3657
dc.language.isoenen
dc.subjectZr–2.5Nb alloyen
dc.subjectDelayed hydride crackingen
dc.subjectThreshold stress intensity factoren
dc.subjectPressure tubeen
dc.titleThreshold stress intensity factor for delayed hydride cracking in Zr-2. 5%Nb pressure tube alloyen
dc.typeArticleen

Click here to download

Original bundle
Now showing 1 - 1 of 1
No Thumbnail Available
Name:
0662.html
Size:
3.91 KB
Format:
Hypertext Markup Language
License bundle
Now showing 1 - 1 of 1
No Thumbnail Available
Name:
license.txt
Size:
1.81 KB
Format:
Item-specific license agreed upon to submission
Description:

Collections